Visit http://www.esabna.com/ for more information about our products.
In an effort to better serve the power generation and petrochemical market segments while improving our delivery on selected Cr.-Mo. alloys, we are discontinuing the sales on 50# HS (hermetically sealed) cans of Atom Arc 8018-B8, 9018-B9 and 9015-B9 product. As we deplete our existing inventory of 50# HS cans and transition to the 10# HS cans we will no longer accept orders for 50# HS cans. In the meantime, we will be building our stock of 10# HS cans to better service the power generation industry.
Our business system has been set up to provide an automatic substitution should you attempt to re-order 50# HS. Please note the various 10# HS part numbers that are affected by this change in packaging. All 10# HS will be packaged as 6 - 10# HS/ carton.
This change does not affect any of our other Atom Arc Cr.-Mo. alloys. We will continue to carry both 50# HS as well as 10# HS on the other popular products.
The following is a list of product part numbers being discontinued. Please take note of these changes for your future orders.
Product Replacement List
| Type | 10# Part No. | 50# HS Part No. |
|---|---|---|
| 8018-B8 3/32" | 255187908 | 255187940 |
| 8018-B8 1/8" | 255187916 | 255187957 |
| 8018-B8 5/32" | 255187924 | 255187965 |
| 8018-B8 3/16" | 255187932 | 255187973 |
| 9015-B9 3/32" | 255061335 | 255061376 |
| 9015-B91/8" | 255061343 | 255061384 |
| 9015-B9 5/32" | 255061350 | 255061392 |
| 9015-B9 3/16" | 255061368 | 255061400 |
| 9018-B9 3/32" | 255067845 | 255067803 |
| 9018-B91/8" | 255067852 | 255067811 |
| 9018-B95/32" | 255067860 | 255067829 |
| 9018-B93/16" | 255067878 | 255067837 |